i_1C 17.5[A/m^2] 1C discharge current Ds_neg 3.9e-14[m^2/s] Solid phase Li-diffusivity Negative Ds_pos 1e-13[m^2/s] Solid phase Li-diffusivity Positive rp_neg 12.5e-6[m] Particle radius Negative rp_pos 8e-6[m] Particle radius Positive T 298[K] Temperature t_plus 0.363 Cationic transport number Dl 7.5e-11[m^2/s] Salt diffusivity in Electrolyte epss_pos 1-epsl_pos-0.259 Solid phase vol-fraction Positive epsl_pos 0.444 Electrolyte phase vol-fraction Positive Ks_pos 3.8[S/m] Solid phase conductivity Positive Ks_neg 100[S/m] Solid phase conductivity Negative cl_0 2000[mol/m^3] Initial electrolyte salt concentration epss_neg 1-epsl_neg-0.172 Solid phase vol-fraction Negative epsl_neg 0.357 Electrolyte phase vol-fraction Negative csmax_neg 26390[mol/m^3] Max solid phase concentration Negative csmax_pos 22860[mol/m^3] Max solid phase concentration Positive cs0_neg 14870[mol/m^3] Initial Negative State of Charge cs0_pos 3900[mol/m^3] Initial Positive State of Charge k_neg 2e-11[m/s] Reaction rate coefficient Negative k_pos 2e-11[m/s] Reaction rate coefficient Positive aA_pos 0.5 Reaction rate coefficient Positive aC_pos 0.5 Reaction rate coefficient Positive aA_neg 0.5 Reaction rate coefficient Negative aC_neg 0.5 Reaction rate coefficient Negative Acell 24e-4[m^2] Cell cross section area i_disch i_1C Discharge current t_disch_stop 2000[s] Discharge duration t_ocp 300[s] Open Circuit interval i_charge -i_1C Charge current t_charge_stop 2000[s] Charge time L_neg 100e-6[m] Length of negative electrode L_sep 52e-6[m] Length of separator L_pos 183e-6[m] Length of positive electrode